Clinical Case: Self-adhesive Cementation of a Zirconia Crown
May 13, 2021 | Dr. Gunnar Reich
About the Case
This 55-year-old female patient presented with an insufficient amalgam filling and fractured enamel on tooth 36. A 3M™ Chairside Zirconia crown was fabricated and seated using 3M™ RelyX™ Universal Resin Cement with a self-adhesive protocol.
Initial situation.
Initial situation (buccal view).
Preparation.
Sandblasting.
Application of 3M™ RelyX™ Universal Resin Cement.
Excess clean-up.
Final situation (buccal view).
Final result.